Abstract
The effect of annealing duration in oxygen flow on the superconducting characteristics of YBa2Cu3O∼7 bulk ceramics was investigated by structural, electrical, magnetic, and electronic microscopy investigations. The long-time annealing is deleterious for the superconductivity in YBa2Cu3O∼7 ceramics. The optimum time interval for annealing is from 20 to 70 h at 950°C, and within this range the maximum value ofT c is obtained.
Similar content being viewed by others
References
J. Jaklovszky and G. Aldica, Proc. of the 2nd Int. Conf. on Thermal Energy Conversion, Texas, 1978.
B. Fischer, J. Genossar, I. O. Jelong, A. Kassel, and J. Ashkenazi,J. Supercond. 1, 53 (1988).
I. Wei Chen, S. J. Keating, X. Wu, J. Xu, P. E. Reyes-Morel, and T. Y. Tien,Solid State Commun. 63, 997 (1987).
M. Popescu, L. Miu, and E. Cruceanu,Philos. Mag. 57, 273 (1988).
T. Graf, G. Triscone, and J. Muller,J. Less-Common. Met. 159, 349 (1990).
P. J. Ouseph and M. R. O'Bryan,Phys. Rev. B 41, 4123 (1990).
J. C. Klem and V. L. Kogan,Jpn. J. Appl. Phys. 26, 3 (1987).
D.-X. Chen and A. Sanchez,Phys. Rev. B 45, 10793 (1992).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Aldica, G., Popescu, M., Popa, S. et al. Sintering time and properties of YBa2Cu3O∼7 superconducting ceramics. J Supercond 8, 365–372 (1995). https://doi.org/10.1007/BF00728173
Received:
Issue Date:
DOI: https://doi.org/10.1007/BF00728173