Thermal stabilities of end groups in hydroxyalkyl terminated polydimethylsiloxane oligomers

  • Published:
Polymer Bulletin Aims and scope Submit manuscript

Summary

Thermal stabilities of α,ω-hydroxypropyl, α,ω-hydroxybutyl, α,ω-2-hydroxypentyl and α,ω-hydroxyhexyl terminated polydimethylsiloxane (PDMS) oligomers were studied. Hydroxypropyl and hydroxybutyl terminated polydimethylsiloxane oligomers showed degradation upon heating, through the loss of functional end groups as determined by FT-IR spectroscopy and gel permeation chromatography. α,ω-Hydroxyhexyl and α,ω-2-hydroxypentyl terminated polydimethylsiloxane oligomers were stable under similar conditions. Instability of the end groups is due to the back biting of the terminal silicon in the PDMS by the primary hydroxyl oxygen, leading to the formation of 5 and 6 membered, stable, heterocylic compounds. Loss of end groups also resulted in a dramatic increase in the molecular weights of the oligomers produced, as determined by gel permeation chromatography.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Author information

Authors and Affiliations

Authors

Additional information

Received: 19 January 1998/Revised version: 27 February 1998/Accepted: 5 March 1998

Rights and permissions

Reprints and permissions

About this article

Cite this article

Yilgor, I., Yilgor, E. Thermal stabilities of end groups in hydroxyalkyl terminated polydimethylsiloxane oligomers. Polymer Bulletin 40, 525–532 (1998). https://doi.org/10.1007/s002890050286