Abstract
The white phosphor matrix 4SrO·7Al2O3 has been synthesized by firing the appropriate mixture of SrCO3, Al(OH)3 and H3BO3 in the molar ratios 1 : 3.5 : 0.135 at 1300°C for 4–7 h. The crystal structure of 4SrO·7Al2O3 has been determined as a orthorhombic Pmma space group with a = 24.7451(2) Å, b = 8.4735(6) Å, c = 4.8808(1) Å, V = 1023.41(3) Å3, Z = 2, and D = 3.66 g cm−3 by the Rietveld analysis. The refinement figures of merit are Rp = 8.26, Rwp = 11.60, Rbragg = 4.44 and s = 2.61 for 844 reflections with 2θ < 119.94°. And the corresponding X-ray powder diffraction data are presented for search/match analysis.
Similar content being viewed by others
References
G. Blasse and A. Bril, Philips Res. Repts. 23 (1968) 201.
V. Abbruscato, J. Electrochem. Soc. 118(6) (1971) 930.
B. Smets, J. Rutten and G. Hoeks, ibid. 136(7) (1989) 2119.
J. T. C. Van Kemenade and G. P. F. Hoeks, Abstract 607, 914, The Electronchemical Society Extended Abstracts, Vol. 83-1, San Francisco, CA, May 8-13, 1983.
Yamamoto Koshi et al., Jpn. Kokai Tokkyo Koho JP 63 191, 886.
Song Qingmei et al., Optics 12(2) (1994) 144.
T. N. Nadzhina, E. A. Pobedimskaya and N. V. Belov, Kristallografiya, 25 (1980) 938.
R. A. Young, "The Rietveld method," Oxford Science Publications, (London, 1993) p. 98.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Wang, D., Wang, M. & Lü, G. Synthesis, crystal structure and X-ray powder diffraction data of the phosphor matrix 4SrO·7Al2O3. Journal of Materials Science 34, 4959–4964 (1999). https://doi.org/10.1023/A:1004759621850
Issue Date:
DOI: https://doi.org/10.1023/A:1004759621850