Effect of CaSO4 Dissolution-Precipitation Time on Formation of Porous Carbonate Apatite as Bone Replacement Material

Article Preview

Abstract:

Introduction: Carbonate apatite type B (C-Ap) has been used as a bone replacement material because of its osteoconductive properties. Clinically, the pores formed in bone replacement material aid in cell mobility and nutrient supply, thereby increasing the bone regeneration ability. CO32- ions found in this material are useful for maintaining a stable physiological environment in the bone in order for it to be easily absorbed by osteoclasts. Porous C-Ap type B is formed using the dissolution–precipitation method by immersing porous anhydrous CaSO4 in a mixture of carbonate and phosphate solutions. Purpose: The present study aimed to evaluate the effect of immersion ofCaSO4using the dissolution–precipitation method on the formation of porous C-Ap type B with calcium sulfate precursor hemihydrate. Method: Porous C-Ap type B was produced usinga mixture of calcium sulfate hemihydrate precursors with 50 wt% polymethylmethacrylate (PMMA) porogen and distilled water. After hardening, the calcium sulfate dihydrate containing PMMA was burned in an oven at 700°C for 4 h to remove the PMMA. The specimen was immersed in a mixture of sodium phosphate (Na3PO4) and sodium carbonate (Na2CO3) for 6, 12, and 24 h. Phase testing through X-ray diffraction (XRD) using CuKα radiation at 40 kV and 40 mA was performed. Attenuated total reflectance-Fourier transform infrared spectroscopy (ATR-FTIR, Thermo Fisher Scientific, Waltham, Massachusetts, USA) was used for detecting the functional groups of CO32- and PO42-. Results: XRD results showed the formation of C-Ap at 6 and 12 h, but the anhydrous CaSO4 phase remained; alternatively, this phase was absent after 24 h of immersion phase andFTIR showed the presence of the functional groups of CO32- compounds. Conclusion: Porous C-Ap type B can be formed from CaSO4 precursors after 24 h of immersion using the dissolution–precipitation method.

You might also be interested in these eBooks

Info:

Pages:

83-90

Citation:

Online since:

February 2020

Export:

Price:

* - Corresponding Author

[1] K. Ishikawa, Bone substitute fabrication based on dissolution precipitation reactions. J Mater. 3 (2010);1138-55.

Google Scholar

[2] E. Landi, G. Logroscino, G. Celotti, A. Tampieri. Carbonated hydroxyapatite as bone substitute. J. Euro. Ceramic Society. 15 (2003):2931-37.

DOI: 10.1016/s0955-2219(03)00304-2

Google Scholar

[3] K. Ishikawa, Y. Miyomato, A. Tsuchiya, et.al.Physical and histological comparison of hydroxyapatite, carbonate apatite, and β-tricalcium phosphate bone substitutes. J Mater. 11(2018):1-12.

DOI: 10.3390/ma11101993

Google Scholar

[4] B.K. Sarma, P. Barman, B. Sarma, A. Das A.R. Pal. Biomimetic deposition of carbonateapatite and role of carbonate substitution on mechanical properties at nanoscale.J. Mater. Letters. 185 (2016):387–88.

DOI: 10.1016/j.matlet.2016.09.028

Google Scholar

[5] S. Nomura, K. Tsuru, M. Maruta, S. Matsuya, I. Takahashi, K. Ishikawa. Fabrication of carbonate apatite blocks from set gypsum based on dissolution-precipitation reaction in phosphate-carbonate mixed solution. J. Dent. Mater.33 (2014): 1–7.

DOI: 10.4012/dmj.2013-192

Google Scholar

[6] K. Ishikawa, Carbonate Apatite Bone Replacement, in A. I.Vasile (ed.), Handbook of Bioceramics and Biocomposites. Springer International Publishing, Switzerland, (2016).

DOI: 10.1007/978-3-319-12460-5_8

Google Scholar

[7] M. Eijken. Human osteoblast differentiation and bone formation: growth factors, hormones and regulatory networks. Haveka BV, Alblasserdam, Netherland, (2007).

Google Scholar

[8] S.T. Li, H.C. Chen, D. Yuen. Isolation and characterization of a porous carbonate apatite from porcine cancellous bone. J. Sci. Tech. Innovation. (2014):1-13.

Google Scholar

[9] I. Sabree, J.E. Gough, B. Derbyn, Mechanical properties of porous ceramic scaffolds: Influence of internal dimensions. J Ceramics Int. 41 (2015):8425–432.

DOI: 10.1016/j.ceramint.2015.03.044

Google Scholar

[10] G. Hannik, J.J Arts. Bioresorbability, porosity, and mechanical strength of bone substitutes: What is optimal for bone regeneration. J Int. Care Injured. 42(2011):22–25.

DOI: 10.1016/j.injury.2011.06.008

Google Scholar

[11] McKenna, Hull. The fire toxicity of polyurethane foams. J Sci. 5(2016);1-27.

Google Scholar

[12] A.Umar, K.J. AbdKarim, N.A. Buang. A review of the properties and applications of poly (methyl methacrylate) (PMMA) polymer reviews. 55(2015):678-705.

DOI: 10.1080/15583724.2015.1031377

Google Scholar

[13] G Hill, Robert.Biomedical Polymer-Biomaterial, artificial organs and tissue engineering.Woodhead Publishing, Swaston.UK, (2005).

Google Scholar

[14] A. Takeuchi, M. Munar, H.Wakae, M. Maruta, S. Matsuya, K.Tsuru, K. Ishikawa. Effect of temperature on crystallinity of carbonate apatite foam prepared from α-tricalcium phosphate by hydrothermal treatment. J.BioMed. Mater.and Eng. 19(2009): 205-11.

DOI: 10.3233/bme-2009-0581

Google Scholar

[15] D. Arsista, Y.K. Eriwati, S. Triaminingsih, Sunarso. Fabrication of porous carbonate apatite based on the dissolution-precipitation of calcium sulfate hemihydrate J. Dentino.4(2019).

DOI: 10.4028/www.scientific.net/kem.829.75

Google Scholar

[16] Anusavice, Kenneth J et. all. Phillips' Science Of Dental Materials, Elsevier Saunders, St. Louis, Missouri USA, (2013).

Google Scholar

[17] F. Daitou, G. Kawachi, M. Maruta, K. Tsuru. Fabrication of carbonate apatite block based on internal dissolution-precipitation reaction of dicalcium phosphate and calcium carbonate.J Dent Mater. 29(2010):303–8.

DOI: 10.4012/dmj.2009-095

Google Scholar

[18] K. Tsuru, A Yoshimoto, M. Kanazawa. Fabrication of Carbonate Apatite Block through Dissolution–Precipitation Reaction Using Calcium Hydrogen Phosphate Dihydrate Block as a Precursor. J Mater 374(2017):1-10.

DOI: 10.3390/ma10040374

Google Scholar

[19] M. Honey, P. Barbara, M.J. Tecklenburg. Carbonate substitution in the mineral component of bone:Discriminating the structural changes, simultaneously imposed by carbonate in A and B sites of apatite. J. of Solid State Chemi.( 2017):25-37.

DOI: 10.1016/j.jssc.2017.07.025

Google Scholar